Difference between revisions of "NIST SRM Certificates"

From Ug11bm
Jump to navigationJump to search
Line 24: Line 24:


===Other NIST SRMs===
===Other NIST SRMs===
*[http://11bm.xray.aps.anl.gov/documents/NISTSRM/NIST_SRM_676b_%5bZnO,TiO2,Cr2O3,CeO2%5d.pdf 676b NIST SRM Certificate for (ZnO,TiO2,Cr2O3,CeO2)]
*[http://11bm.xray.aps.anl.gov/documents/NISTSRM/NIST_SRM_674b_%5bZnO,TiO2,Cr2O3,CeO2%5d.pdf 676b NIST SRM Certificate for (ZnO,TiO2,Cr2O3,CeO2)]


===NAC===
===NAC===
Na2Ca3Al2F14 (NAC) is not a official SRM, but can be used as a low Z sharp line profile standard with strong peaks at lower 2theta (compared to LaB6)
Na2Ca3Al2F14 (NAC) is not a official SRM, but can be used as a low Z sharp line profile standard with strong peaks at lower 2theta (compared to LaB6)
*[http://11bm.xray.aps.anl.gov/data/standards/NAC/11BM_NAC.cif CIF file for NAC] <small>''Note: see CIF text file header for more info about NAC sample'' </small>
*[http://11bm.xray.aps.anl.gov/data/standards/NAC/11BM_NAC.cif CIF file for NAC] <small>''Note: see CIF text file header for more info about NAC sample'' </small>

Revision as of 16:23, 13 November 2013

These files are provided for the convenience of APS beamline 11-BM users.

We do not guarantee or endorse these SRM materials.

See the NIST page for more details http://www.nist.gov/srm/

Al2O3

LaB6

Si

Other NIST SRMs

NAC

Na2Ca3Al2F14 (NAC) is not a official SRM, but can be used as a low Z sharp line profile standard with strong peaks at lower 2theta (compared to LaB6)